Crystals Materials

CLBO Crystal Growth and Performance

clbo-crystal-growth-and-performance
CLBO Crystal Growth and Performance

Growing CLBO

CLBO (CsLiB6O10) is grown from melt by techniques such as the top-seeded solution growth method. Achieving the large, inclusion-free, low-absorption boules needed for high-power deep-UV conversion demands tight control of melt stoometry, growth temperature and cooling — defects and inclusions directly raise absorption and lower the damage threshold that makes CLBO valuable. AOG controls the full growth-to-polished-crystal process in-house.

What "performance" means for CLBO

Performance factorWhy it matters
Optical homogeneity / low inclusionsLow absorption → less heating and higher DUV output
Deep-UV transmissionEfficient 266 nm and shorter-wavelength generation
Damage thresholdSurvives the high fluence of 4th-harmonic generation
Surface quality (flatness, scratch-dig)Preserves beam quality at the conversion faces
Moisture handlingCLBO is hygroscopic — dry, temperature-stabilised packaging protects it

From boule to coated crystal

After growth, CLBO is oriented, cut to the phase-matching angle for 266 nm (or the target DUV wavelength), polished to tight flatness and scratch-dig, and AR-coated. Because CLBO is hygroscopic, the finished crystal is housed in a dry, temperature-controlled cell. See our CLBO product page and the CLBO deep-UV article.

Frequently asked questions

Why does CLBO quality vary? Growth defects and stoichiometry deviations raise absorption and lower damage threshold; tight growth control is essential.

How is CLBO protected from moisture? It is kept in a dry, temperature-controlled housing, since it is markedly hygroscopic.

Can CLBO be grown to large aperture? Yes — large, high-quality CLBO crystals are achievable and are used for high-power 266 nm stages.

For more information on crystal materials, please consult info@aogcrystal.com